Originally Posted by FunctionalShaker View Post
Thing is, the short leaves needed to be sand blasted and I've blasted the second leaves to remove the black paint and stains that came from Eaton. I was planning on epoxy priming each leaf separately then reassembling the springs and painting.

Don't you have a hard time keeping parts clean that are coated in cosmolene?
Not at all. recently blasted metal will almost soak up the cosmolene. The mil grade will actually harden in temps<65f or so. I use a cheap heat gun on the pint size can, turns it to liquid almost immediately,use cotton rags and soak it on.