Hi Mr. Reid and Musclcah...Thanks for the recommendations on the filler to use. I haven't done this sort of work in a long time...so I'm figuring on steep learning curve catching up on 30 years or so of development.
With regard to lead work: It was really interesting to watch the process. It looked like quite the balancing act between keeping the body metal hot enough and the lead short of the temperature where it would just run.
Thanks again to everyone for their input and interest.