Weld both sides. Grind and clean the crack 1/8 deep or more. Wire brush it with a stainless steel wire brush only. Do not grind the weld off. Pack a wet rag around the shaft area to keep it cool. After it is welded and I mean just after, take a water hose and flash cool the weld to temper it back to T6 temper.
And go have fun.