I emailed the place where I bought it and got a response but it didn’t answer the question. Didn’t even come close! I’m thinking that somehow the mixing was incomplete because I had areas that sanded with no pick up but yet it setup quick as I could only skim half a roof before I had to mix another batch. I say that it set up quick but really I spent more time mixing than I did spreading it.
The All-Metal Filler must be sanded down with 60 or 80 grit paper, most people use an air hi-speed sander. The product is designed to fill in and seal the area from water. It should then have a thin coat of body filler applied over the All-Metal. Once dry, the body filler can then be sanded smooth. If you have any more questions, please contact our tech department
at 1-800-321-9260.
TP Tools
|