Quote:
Originally Posted by HWYSTR455
Uhg. Never use generic or 'house' paint on car stuff, but guess you know that now.
SEM makes products for prepping and spraying plastic parts, do your homework, SEM has resources available to study.
https://www.semproducts.com/
It's generally a 3 step process, clean, promoter, and paint.
.
|
Uhg was milder than my reaction, but yes, Uhg
As for the Krylon vs SEM, was following OP's example, which clearly worked great for him.
My results were different.
Now that I've established my plastic is hard to wet, I'll follow your advice and go get some SEM products. I have an adhesion promoter already and see that SEM makes a gloss black aerosol. My Summit prep solvent did not eat the plastic, which was good, but maybe the SEM prep solvent would be better ??