Quote:
Originally Posted by Tom Vaught
Not sure about Camshafts and the correct order to Nitride them, Paul, BUT I HAVE HAD OVER 15 CRANKSHAFTS NITRIDED BY MOLDEX AFTER THEY WERE MACHINED. Joe (and Whitey when he was alive) said Nitriding was the last step. I believe them.
Never had a failure of the crank yet.
Tom V.
|
I agree Tom. The Nitrided cams we get from Crower were finished ground and shipped in with their crankshafts to be done. When we order them from Competition Cams and the place that grinds our "house" cams they told me their process is to rough grind, Nitride then finish grind. Also Comp charges for "custom grind" when you Nitride one of their "catalog" cams.