All " cadmium " Gold looking items are coated, not electrically, On Top Of a silver " ZINC" coating that Is electrically done.
Sodium BiChromate in a sulfuric acid solution is used after the Silver Zinc is done to get the Gold look.
IT IS NOT Gold " Cadmium".
I do this on Alt Pulleys and booster shells, BUT. I don't have a container long enough for a jack mast to zinc it or one that long to get the Gold on it after.
I used to buy my Bi chromate in bulk from Russia. There are some smaller amounts sold still in the US.

__________________
"The Future Belongs to those who are STILL Willing to get their Hands Dirty" .. my Grandfather