You need to neutralize it with water after you're done dipping.

Naval jelly is another form of phosphoric acid in a jelly carrier so that you can apply it to vertical surfaces. Personally, I would sand blast an exterior panel like that.

Another hint on the dipping, periodically take the part out and brush the rust off with a stiff bristle brush. This will quicken the process.

John

__________________
1967 Firebird Convertible Factory 400/4spd
Now 462/5spd Fuel Injected
http://1967firebird.atwebpages.com/
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 03:16 PM.

 

About Us

The PY Online Forums is the largest online gathering of Pontiac enthusiasts anywhere in the world. Founded in 1991, it was also the first online forum for people to gather and talk about their Pontiacs. Since then, it has become the mecca of Pontiac technical data and knowledge that no other place can surpass.

 




Copyright © 2017