The early 59-61 forged rods have a chance to be heat treated with the right person doing it. Butler had a guy many years ago who could bring them up to the high 20s/low 30-31 range. Never to 421 SD numbers. The guy eventually passed. RIP.

The 'Rubber Rods' ~61 to 63+ vintage are softer than the cast iron rods and will waste your money even trying to heat treat them. Even the poorest Chinese rods will typically test out better than the rubber rod stuff but the rubber rods had at least minimal clean steel.

Cast rods are great, as is any "hard material" rod is, (until they fracture).

Tom V.

__________________
"Engineers do stuff for reasons" Tom Vaught

Despite small distractions, there are those who will go Forward, Learning, Sharing Knowledge, Doing what they can to help others move forward.
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:07 PM.

 

About Us

The PY Online Forums is the largest online gathering of Pontiac enthusiasts anywhere in the world. Founded in 1991, it was also the first online forum for people to gather and talk about their Pontiacs. Since then, it has become the mecca of Pontiac technical data and knowledge that no other place can surpass.

 




Copyright © 2017